Epoxy is the glue, filler and resin for most repairs on a timber or fibreglass boat. Mixed as it comes it's a resin, for sealing timber and wetting out fibreglass. Thickened with a filler powder it becomes a glue or a filler. It has to be mixed in the right ratio and mixed well, and it goes off faster the more of it is left sitting in the pot, so mix small amounts. I wear gloves, because repeated contact can make your skin more sensitive to it.
In this video I cut a patch of rot out of a catamaran's deck and make a new piece from ply. I coat all the exposed timber and the patch with Everdure, a very thin epoxy that seals the timber, and leave it until it no longer smells before going on. Then I glue and screw the patch in with epoxy thickened to peanut butter consistency, so it stays on the edges instead of dripping into the boat, and glass over it in staggered sheets, like courses of bricks, to build up the low spots rather than relying on fairing compound.
Filling cracks and gouges
On the same catamaran, cracks and deep gouges where a mooring rope had rubbed the rudder and bow. I wipe them with methylated spirits to draw out moisture, seal them with Everdure, then while that's dry but not fully gone off, fill them with West System epoxy and chopped fibreglass for a good chemical bond.
Glassing over a hole
A hole with a dowel in it through the bottom of a putt-putt's hull, with no sign of it outside. I wipe it out with acetone, then glass over it with discs of fibreglass, brushing on resin until the glass goes clear; the dowel will be fine once it's soaked in epoxy. Only two to four layers can go on at once because of the heat it makes as it goes off, and more layers need to go on within about four hours. After that you get amine blush on the surface and have to clean and sand it for a mechanical bond. Over three days that built up to 12 layers, which I ground flat before one last patch over the top.
Laminating a plywood transom
Gluing two sheets of ply together for a transom. The epoxy is mixed thoroughly before adding the Cab-O-Sil, and thickened to a jelly consistency, thick enough to fill gaps but thin enough to squeeze out when it's clamped. Spread thin it goes off more slowly than in the pot, where the heat builds up. Screws with a smooth shank above the thread clamp the sheets together; fully threaded screws just hold them apart.
Metering, thickening and wetting out
Gluing and glassing payson butt joints in plywood. The West System pumps meter the five to one ratio with one pump of each, and alternating them keeps the ratio right even if you lose count. I thicken the epoxy with Cab-O-Sil into a glue, then brush resin onto the fibreglass until it turns from white to clear and roll out the air bubbles.