Paint on a steel boat is there to keep water and salt away from the metal. The usual system is an epoxy primer straight after blasting, epoxy filler, epoxy barrier coats that do most of the protecting, then polyurethane above the waterline and antifoul below it. Fix the rust and holes first; see repairing a steel hull and removing rust.
In this video Dave from Altex talks me through their system for the trawler: blast it, get the epoxy primer on within four hours, then epoxy filler, barrier undercoats and a high build surfacer if needed, with the antifoul going on over the last barrier coat the same day. Then the hull is sandblasted. I wash it down with Hold Blast in the pressure washer to stop flash rust, and roll the epoxy primer onto the good steel, leaving the spots that still need welding for later.
Single pack for easy touch-ups
Years later, finishing Renko's deck, I still use two-pack epoxy for the primer and barrier coat, but in this video I switch to a single-pack topcoat, Norglass slip-resistant deck paint, with a little Penetrol because the old gloss finish is still a bit smooth even after sanding. The truth is I never touched up the two-pack paint that was on originally. With single pack I can just open the tin and touch up the blue and the deck more often, and I want to see whether that's a better way to go with a steel boat.
Topcoats on the hardstand
The spots where the hull sat on its pads weren't sandblasted, and the epoxy fell off them easily. In this video I rough them up with a tungsten-tipped Turco wheel and prime them again. Then high build epoxy primer goes on the outside, I sand the old urethane topcoat so the new one keys into it, and the deck and the inside of the bulwarks get a very thick, tough two-pack light grey paint.
Filler and coats
Marks on the blasted steel after rain, epoxy spot filler over the pitting, and sanding it smooth. Then Dave comes back to explain the timing between coats: the barrier coat can go on two hours after the primer, but no more than two coats a day or solvent gets trapped. He shows how a wet film thickness gauge tells you how much paint you're putting on: about half of it is solvent, so 200 microns wet leaves 100 dry, and you want 300 to 400 microns of epoxy below the waterline and at least 150 above it. And polyurethane goes over the epoxy because it stands up to UV and keeps its colour and gloss. Then two barrier coats go on.